The cover rubber mainly used for hot vulcanization conveyor belt joints and seams, it has good features of wear resistant and corrosion resistant after hot vulcanized. The cover rubber should be used together with intermediate rubber.
Polymer: NR / CR
Specific weight: 1.12 +/-0.03 g/cm3
Hardness: 65+/-3 shore a
Abrasion: 140 mm3 at 10 N
Tensile strength: > 20 MPA
Elongation at break: > 600 %
Curing temperature: 145 - 160 ℃
Order No. |
Thickness / mm |
Width / mm |
Weight / roll |
701011 |
1 |
500 |
10 kg |
701012 |
2 |
500 |
10 kg |
701013 |
3 |
500 |
10 kg |
701014 |
4 |
500 |
10 kg |
701015 |
5 |
500 |
10 kg |
701016 |
6 |
500 |
10 kg |
701017 |
7 |
500 |
10 kg |
701018 |
8 |
500 |
10 kg |
701021 |
1 |
1000 |
20 kg |
701022 |
2 |
1000 |
20 kg |
701023 |
3 |
1000 |
20 kg |
701024 |
4 |
1000 |
20 kg |
701025 |
5 |
1000 |
20 kg |
701026 |
6 |
1000 |
20 kg |
701027 |
7 |
1000 |
20 kg |
701028 |
8 |
1000 |
20 kg |